    How to control and prevent internal cracking (honeycomb cracking) in wood

    Internal wood cracking occurs inside the wood, cracking along the wood rays, such as honeycomb, also called honeycomb cracking. There are no cracks on the surface, only sawing can be found. But it is usually accompanied by uneven appearance or significant shrinkage, or charring, or lighter weight. This is characteristic of over-drying.

  • 2809-2022

    How to control and prevent wood cracking

    Surface cracks are longitudinal cracks that occur along the wood rays on the outer surface of sawn timber (usually the outer cut surface of a chord-cut board). It is caused by excessive surface tensile stress in the early stage of drying

  • 0509-2022

    Wood drying: "Natural" is the best

    "Natural is the best." In modern society, this has almost become a consensus of people. Everyone knows the reason: modern technology is used in various fields, and almost all products are linked to technology, so that natural things are becoming more and more scarce, and people are beginning to miss the "natural gas" that can be seen everywhere. good time.

  • 2908-2022

    Thermal modification of wood modification (wood heat treatment)

    Wood modification is the process of improving the properties of wood. It uses chemical, biological or physical media to act on the wood to enhance the desired properties of the wood during the service cycle. In addition, the modified wood itself should be non-toxic during the service cycle and not release any toxic substances during or after the service cycle.

  • 1708-2022

    Prevention and Control of Wood Blue Staining

    How to prevent and control the blue of wood? Is there a good way?

  • 0506-2023

    Convective drying of wood in gaseous media - factors affecting wood drying speed

    Factors Affecting Wood Drying Speed The main factors affecting the drying speed of wood are medium temperature, humidity, air circulation speed, wood moisture content gradient, and temperature gradient.

  • 2905-2023

    Convective drying of wood in a gaseous medium – movement of internal moisture as wood dries

    Moisture in wood can move inside the wood under certain conditions, which is called moisture conductivity of wood. Moisture can drain from both ends of the wood by moving along the fiber direction, or it can drain from the sides of the wood across the fiber direction, and in most boards, the length is much greater than the thickness width. The side area of ​​the sheet is much larger than the end area. Therefore, although the conduction of moisture along the fibers is easier than that across the fibers, it is the conduction across the fibers that plays a decisive role in wood drying.

  • 2405-2023

    Convective drying process of wood in gaseous medium - wood drying curve

    wood drying curve When the wood is dried in a gaseous medium with a certain temperature and humidity, if the change of the moisture content of the wood is measured at regular intervals, and the time is taken as the abscissa and the moisture content is drawn on the ordinate, the curve is called the drying curve. (Figure 1-2). The drying process can be analyzed on the drying curve diagram. The whole process of wood drying can be divided into three stages.

  • 1110-2023

    Introduction to Track Type Veneer Drying Kiln

    The track type veneer kiln is a patented veneer drying equipment independently developed by our company. The following is a comparison of the advantages and disadvantages between track type veneer drying kilns and roller type dryers

Get the latest price? We'll respond as soon as possible(within 12 hours)

Privacy policy